- Description
High Heat Resistance Tin Silicone Rubber
Designed specifically for casting metals
Heat resistance is 565F
Parts A & B are mixed 100A & 3B by weight
Pot life is 40 minutes and cure time is 24 hours
Designed specifically for casting metals
Heat resistance is 565F
Parts A & B are mixed 100A & 3B by weight
Pot life is 40 minutes and cure time is 24 hours